PU Isolating filler DP 4784-9343
Hesse PU Isolating filler DP 4784-9343 is a primer for the highest isolating effect and quality requirements. This product is ideally suited for use beneath Hesse high gloss lacquers and features great machine sanding capability.
Enquire articlePage content
- especially good machine sanding capability
- optimum tendency not to run under high gloss
- extremely wide range of applications
Processing
Areas of application
For all interior fixtures and fittings, including high demand areas such as kitchens and bathrooms.
Technical information
Certificates
Technical Specifications
Proportion of renewable raw materials % | 0 % |
---|---|
Appearance | opaque |
VOC EU % | 34 % |
Number of layers (max) | 4 |
Quantity per layers (min) | 140 g/m² |
Quantity per layers (max) | 300 g/m² |
Total quantity applied | 800 g/m² |
Mixing ratio (volumetric) | 5 : 1 | Hardener: DR 4052 |
Mixing ratio (gravimetric) | 100 : 16 | Hardener: DR 4052 |
Processing Instructions
Potlife | 2 h / 20 °C |
---|---|
Drying | 5 h / 20 °C |
Due to hardening | 7 d / 20 °C |
Stackable according to | 16 h / 20 °C |
Surface sanding (grain size) | 150 - 320 |
Intermediate sanding (grain size) | 320 - 400 |
Yield per pass | 5 - 10 m²/l |
Processing information | One- to four-coat application at 100 - 300 g/m² on suitable substrates, maximum application amount in wet film: 800 g/m².Prescribed sanding of the suitable substrate / dust removal. Intermediate sanding at 280 - 400 grit / dust removal . |
Special notes | For MDF substrates: With MDF coatings, you can avoid painting faults and edge breaks if you observe the following: Selection of an MDF quality suitable for the field of application, see manufacturer data on EU standard EN 622-5 pt.4 Test methods EN 317 (requirements on thickness swelling). Ideal panel moisture 5 - 7 %. If possible coat the MDF all around, the backs should at least receive a clear coating. Avoid sharp edges and milling grooves, round-off wherever possible. Coat edges and milling grooves 2 x with primer, do not sand through, if need be, prime again. Thick boards that have been built by gluing together several thinner boards are, due to the variance in tension, susceptible to edge ridging. It is better to select a single MDF board of the appropriate thickness. Panels that have been glued together should always be sanded flat at the edges and colourlessly pre-insulated. Any water introduced by the gluing process must be allowed to evaporate prior to coating. Store filler-coated surfaces in an air conditioned location and apply the final coat in a timely manner. |
Procedure example
Our technical information is continually adapted to keep up to date with the latest technology and statutory regulations. The latest version is always available online at www.hesse-lignal.de or talk to your local account manager. This information is for advice and is based on the best knowledge available and careful research in line with the current state of the art. This information cannot be held as legally binding. We also refer you to our terms and conditions of business. Safety data sheet is provided in accordance with EC regulation no. 1907/2006.